Fabrication method for molybdenum disilicide sintered body
US5907760A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Mar 31, 1997 |
| Grant date | May 25, 1999 |
| Priority date | — |
| Expiry date | Mar 31, 2017 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C29/18
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A fabrication method for a molybdenum disilicide sintered body in which a molybdenum disilicide powder having excellent oxidation resistance is sintered in a low-temperature sintering method and compacted at a low temperature and under no pressure, includes carrying out a milling on a molybdenum disilicide powder at a low temperature, providing a diffusion path required to sinter the molybdenum disilicide on which a milling is performed, and sintering the resultant powder under the atmosphere of hydrogen or argon gas.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.