Pourable cast melt bar compositions comprising low levels of water and minimum ratios of polyol to water

US5916856A · kind A · utility

18Cited by
6References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 16, 1996
Grant dateJun 29, 1999
Priority date
Expiry dateOct 16, 2016

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC11D3/2065
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

The present invention relates to cast melt bar composition comprising surfactant, fatty acid, generally lower MW polyalkylene glycol and small amounts of water wherein the ratio of total polyol to water is at least 3:1. By using less water and greater variants of polyol, the bars allow larger amounts of generally insoluble materials to be used and also allow retention of bar integrity using limited amounts of soap (important for mildness).