Manufacture of a metal bonded abrasive product
US5932508A · kind A · utility
Inventors
Key dates
| Filing date | Sep 3, 1997 |
| Grant date | Aug 3, 1999 |
| Priority date | — |
| Expiry date | Sep 3, 2017 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S76/12
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of manufacturing a metal bonded abrasive product such as a saw or drill segment or bead for a diamond wire is provided. The method includes the steps of providing a mixture of the metal, in particulate form, and the abrasive particles, cold pressing the mixture to the desired final shape at a pressure in the range 320 to 1500 MPa to produce a cold pressed product at a temperature in the range 900 to 1300.degree. C. under conditions which inhibit degradation of the abrasive particles and the particulate metal. The product, after free sintering, will generally have a relatively high porosity, for example, a porosity of 10 to 25 percent by volume.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.