Hexagonal system ferrite particles and their production process
US5945028A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Mar 6, 1997 |
| Grant date | Aug 31, 1999 |
| Priority date | — |
| Expiry date | Mar 6, 2017 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH01F1/11
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A slurry containing ferrite magnet raw material particles and a non-aqueous solvent is compacted wet in a magnetic field, while said non-aqueous solvent is removed therefrom, to obtain a compact, and the compact is sintered to obtain an anisotropic ferrite magnet. In this case, a surface active agent is allowed to exist in the slurry during the wet compaction. Alternatively, in addition to or in place of this, the raw material particles are pulverized to apply strains thereto, thereby reducing the iHc values to preferably 3.5 kOe or less. This makes some considerable improvement in the degree of orientation of the compact, thus achieving much more improved magnet properties.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.