Air bag made of silicone modified thermoplastic polyurethane resin
US5945185A · kind A · utility
24Cited by
2References
8Claims
0Family size
Assignees
Inventors
Key dates
| Filing date | Jun 15, 1998 |
| Grant date | Aug 31, 1999 |
| Priority date | — |
| Expiry date | Jun 15, 2018 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/1345
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
An air bag made of thermoplastic polyurethane resin which can be deployed quickly enough over a wide range of temperature from very low to high and which can exhibit stable performance without danger of blocking is made of silicone modified thermoplastic polyurethane resin in which the content of siloxane is 5-40% by weight. An occupant can be protected by the air bag over a wide range of temperature such as from -40.degree. C. to +100.degree. C.