Abstract

A method for recovering rare earth elements and cobalt from a rare earth-iron alloy containing cobalt is disclosed, including the steps of: PA1 a preparing a slurry of the rare earth-iron alloy containing cobalt, PA1 adding a diluted nitric acid solution to the slurry with air being introduced into the slurry, while maintaining pH of a resulting mixture at 5 or higher to dissolve metals including rare earth metals and cobalt at 50.degree. C. or lower, and PA1 separating an undissolved residue containing iron from a rare earth-containing nitrate solution by filtration.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.