Process for producing crystalline ceric oxide particles and abrasive
US5962343A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 24, 1997 |
| Grant date | Oct 5, 1999 |
| Priority date | — |
| Expiry date | Jul 24, 2017 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2006/12
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
According to the present invention, a process is provided for producing crystalline ceric oxide particles having a particle diameter of 0.005 to 5 .mu.m, which comprises the steps of reacting a cerium (III) salt with an alkaline substance in an (OH)/(Ce.sup.3+) molar ratio of 3 to 30 in an aqueous medium in an inert gas atmosphere to produce a suspension of cerium (III) hydroxide, and blowing oxygen or a gas containing oxygen into the suspension at a temperature of 10 to 95.degree. C. and at an atmospheric pressure.