Patent · US Expired

Method for recovering reusable elements from rare earth-nickel alloy

US5980841A · kind A · utility

11Cited by
0References
14Claims
0Family size

Assignee

Inventor

Key dates

Filing dateFeb 11, 1997
Grant dateNov 9, 1999
Priority date
Expiry dateFeb 11, 2017

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02W30/84
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for recovering reusable elements including rare earth elements from a rare earth-nickel alloy is disclosed, including the steps of: PA1 preparing a slurry of the rare earth-nickel alloy, PA1 adding a diluted nitric acid solution to the slurry over a period of time under stirring at a temperature not higher than 50.degree. C. while maintaining pH of a resulting mixture at 5 or higher to dissolve soluble metals including rare earth metals, and PA1 separating an undissolved residue containing nickel from a rare earth-containing nitrate solution by filtration.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.