Prosthetic restoration and manufacturing method thereof
US5984683A · kind A · utility
Assignees
Inventors
Key dates
| Filing date | Jan 20, 1998 |
| Grant date | Nov 16, 1999 |
| Priority date | — |
| Expiry date | Jan 20, 2018 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S623/924
- WIPO fieldPharmaceuticals
- WIPO sectorChemistry
Abstract
A prosthetic restoration of the invention is made from a metal material containing Ti as the main component and from 0.01 to 3 wt % of M (were M is at least one element selected from the group comprising Si, Zr, Ca, P and In). Further, in addition to these materials, from 0.01 to 4 wt % of Q (where Q is at least one element selected from the group comprising Al, Sn, V ad Cu) may be contained. On an outer surface of such a metal material, a coating layer formed of porcelain or synthetic resin or the like can be provided. Such a prosthetic restoration can be manufactured as follows. First, a model of an abutment tooth is manufactured. Next, a compound is prepared by mixing and kneading metallic powder of Ti or an alloy containing Ti, powder composed of the M or a compound containing the M and a binder. In this case, the powder composed of Q or an compound containing the Q may be added. Thereafter, thus obtained compound is built up onto the model of the abutment tooth to form a green body of the prosthetic restoration having a desired shape. Here, it is preferred that the built-up mass becomes slightly larger than the desired shape taking shrinkage of the built-up mass during sinteri…
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.