Abstract

The present invention provides a hollow oxide particle including a shell wall constituting a hollow room, and the shell wall has a thickness of 20 nm or less. The shell wall may be mainly composed from at least one selected from the group consisting of alumina, spinel, iron oxides, yttrium oxides, and titanium oxides. A process for producing the hollow oxide particle comprises the steps of: forming a Water in Oil (W/O) type emulsion including aqueous microspheres having a each diameter of 100 nm or more, by adding an organic solvent to an aqueous solution dissolving and/or suspending at least one of metal salts and metal compounds; and forming the hollow oxide particle by atomizing the Water in Oil (W/O) type emulsion to burn. When the hollow oxide particle is brought into contact with a water-containing solution, a surface of the shell wall may have a minutely irregular surface.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.