Process for conditioning a gas-phase reactor to produce an ethylene-propylene or ethylene-propylene-diene rubber
US6011128A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jun 17, 1998 |
| Grant date | Jan 4, 2000 |
| Priority date | — |
| Expiry date | Jun 17, 2018 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S526/901
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
There is provided process for producing an ethylene-alpha-olefin polymer at a polymerization reaction temperature in excess of the softening temperature of the polymer in a gas-phase fluidized-bed reactor in the presence of a polymerization catalyst and wherein the polymerization reaction is conducted in the presence of an inert particulate material, the improvement comprising: commencing polymerization by polymerizing an ethylene propylene rubber having a crystallinity ranging from about 4 to 18 percent as measured by differential scanning calorimetry.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.