Method for sliver elimination in shearing aluminum sheet

US6045636A · kind A · utility

7Cited by
4References
6Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMay 15, 1997
Grant dateApr 4, 2000
Priority date
Expiry dateMay 15, 2017

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/057
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Age-hardened aluminum alloy sheet can be subjected to a shearing operation, such as trimming or piercing, with reduced sliver formation by first heating the region to be sheared to a temperature above about 250.degree. C., immediately quenching the heated region to soften the region, and then performing the shearing operation in the softened region before age-hardening occurs.