Method of brazing directionally solidified or monocrystalline components
US6050477A · kind A · utility
9Cited by
11References
12Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 31, 1998 |
| Grant date | Apr 18, 2000 |
| Priority date | — |
| Expiry date | Mar 31, 2018 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB23K1/002
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
In a method of brazing directionally solidified or monocrystalline components, the brazing deposit and the directionally solidified or monocrystalline component are moved through a heated zone. In this zone, the temperature applied by a heating system is greater than the liquidus temperature of the brazing alloy and less than the local incipient melting temperature of the component. A thermal gradient is applied between the component and the brazing deposit.