Method of pipe welding

US6093906A · kind A · utility

29Cited by
4References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 23, 1999
Grant dateJul 25, 2000
Priority date
Expiry dateJul 23, 2019

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB23K2101/06
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

A method of welding the ends of two pipes at the open root between the spaced ends by an STT electric arc welder, which comprises: selecting a welding wire having 0.06-0.15% by weight carbon, 0.90-1.40% by weight manganese, and 0.45-0.75% by weight silicon, as well as phosphorous, copper, stainless steel alloys and sulfur; maintaining the sulfur at a given percentage level of the selected wire in the specific range of 0.015 to 0.035% by weight; and maintaining said phosphorous at a given percentage level of said selected wire in the specific range of less than about 0.015%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.