Patent · US Expired

Method for the manufacture or repair of a blisk by linear friction welding

US6095402A · kind A · utility

43Cited by
10References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 22, 1998
Grant dateAug 1, 2000
Priority date
Expiry dateJun 22, 2018

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49318
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

A method of making a BLISK by linear friction welding, comprises providing a stub on the circumferential surface of a turbine disk and defining a weld joint surface on the radially outermost face of the stub. The weld joint surface follows the annulus curvature in axial and circumferential directions while remaining flat in a third direction. A blade is applied radially to the stub and linear friction welding of the blade to the stub is effected by oscillating the blade in said third direction while applying a welding force inwardly along the blade.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.