Process for manufacture and use of improved attrition resistant catalyst
US6107238A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Sep 30, 1998 |
| Grant date | Aug 22, 2000 |
| Priority date | — |
| Expiry date | Sep 30, 2018 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S502/504
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
A method for manufacturing of an improved attrition resistant catalyst having an oxide-rich surface layer involving forming a slurry comprising; catalyst, catalyst precursor or catalyst support particles (e.g., transition metal oxides), a colloidal oxide sol (e.g., colloidal silica), and a solution of a solvent and solute wherein the solute consist essentially of a precursor of said oxide-rich surface with particle size no greater than 5 nm (e.g., aqueous silicic acid or polysilicic acid) and then spray drying the slurry to form porous microspheres of attrition resistant catalyst; and, calcining the spray dried microspheres. Such a catalyst is particularly useful in oxidation processes wherein the oxidation is performed by an oxidized form of the catalyst and the resulting reduced form of the catalyst is separately regenerated (e.g., two-step vapor phase processes carried out in recirculating solids reactors, transport bed reactors or circulating fluidized bed reactors and the like).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.