Patent · US Expired

Process for the production of anisotropic ferrite magnets and anisotropic ferrite magnets as well as hexagonal system ferrite particles and their production process

US6132635A · kind A · utility

5Cited by
17References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 19, 1999
Grant dateOct 17, 2000
Priority date
Expiry dateMar 19, 2019

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01F1/11
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

ferrite magnet raw material particles and a non-aqueous solvent is compacted wet in a magnetic field, while said non-aqueous solvent is removed therefrom, to obtain a compact, and the compact is sintered to obtain an anisotropic ferrite magnet. In this case, a surface active agent is allowed to exist in the slurry during the wet compaction. Alternatively, in addition to or in place of this, the raw material particles are pulverized to apply strains thereto, thereby reducing the iHc values to preferably 3.5 kOe or less. This makes some considerable improvement in the degree of orientation of the compact, thus achieving much more improved magnet properties.