Calcium silicate board and method of manufacturing same

US6139620A · kind A · utility

17Cited by
2References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 18, 1998
Grant dateOct 31, 2000
Priority date
Expiry dateFeb 18, 2018

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02W30/91
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of manufacturing a calcium silicate board having a bulk specific gravity of approximately 0.5 to 0.8, which method achieves a decrease in the bulk specific gravity and an increase in the matrix strength of the board without impairing productivity, and the calcium silicate board obtained by this method. The method is characterized in that a material slurry comprising 5 to 30 wt % of calcium silicate hydrate slurry as a solid component, 17 to 50 wt % of calcareous material, 13 to 45 wt % of silica containing material, 2 to 8 wt % of fiber material, and 5 to 40 wt % of inorganic fillers is formed through conventional processes and the obtained molded body is subjected to a hydrothermal reaction in a pressure container.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.