Highly corrosion and wear resistant chilled casting
US6165288A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Nov 18, 1996 |
| Grant date | Dec 26, 2000 |
| Priority date | — |
| Expiry date | Nov 18, 2016 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/12799
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A chilled casting is characterized by high corrosion resistance in aggressive media and by a wear resistance that approaches that of commercially available types of chilled casting. The disclosed chilled casting contains 36 to 46% by weight Cr, 5 to 12% weight Ni, 2 to 6% by weight Mo, up to 3% by weight Cu, up to 0.2% by weight N, up to 1.5% by weight Si, up to 1.5% by weight Mn and 1.4 to 1.9% by weight C, the remainder being Fe and impurities due to the production process. The chilled casting further contains 20 to 40% by volume austenite, 20 to 40% by volume ferrite and 20 to 40% by volume carbides having a lattice structure.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.