Process to produce low density polymer in a loop reactor
US6166152A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Feb 26, 1998 |
| Grant date | Dec 26, 2000 |
| Priority date | — |
| Expiry date | Feb 26, 2018 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S526/943
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method for producing a low density copolymer of ethylene and 1-hexene having a density in the range of about 0.915 to about 0.930 grams/cc in a continuous loop reactor under slurry phase reactor conditions in the presence of a liquid diluent comprising (a) using a prepolymerized solid particulate metallocene catalyst system, (b) combining the catalyst system with a liquid diluent, and (c) agitating the mixture of (b) to form a liquid mixture containing catalyst system particles that are substantially uniform in size, (d) passing this liquid mixture into the loop reactor, (e) not adding any hydrogen, (f) employing the temperature in the range of about 170.degree. F. to about 180.degree. F., (g) employing ethylene in an amount equal to about 5 to about 6 weight % of the liquid diluent and the loop reactor, and (h) employing 1-hexene in an amount equal to about 1.5 to about 2.5 weight % of the liquid diluent in the loop reactor.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.