Patent · US Expired

Acid pretreatment for adhesive bonding of vehicle assemblies

US6167609A · kind A · utility

17Cited by
22References
12Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 26, 1997
Grant dateJan 2, 2001
Priority date
Expiry dateDec 26, 2017

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49982
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

An aluminum alloy sheet, plate, casting or extrusion having a surface layer containing magnesium oxide and aluminum oxide is cleaned with an acidic solution. The cleaned component has an aluminum oxide layer that is pretreated with a phosphorus-containing organic acid to form a functionalized layer. A layer of polymeric adhesive is applied to the functionalized layer, and the adhesive layer is joined to a metal support structure to form a vehicle assembly.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.