Patent · US Expired

Corrosion resistant ceramic and a production method thereof

US6200918A · kind A · utility

18Cited by
12References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 15, 1998
Grant dateMar 13, 2001
Priority date
Expiry dateDec 15, 2018

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01J61/302
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A TAG, LAG or YbAG anti-corrosion layer of which Si content is 100 ppm or under and total content of Ca and Mg is 200 ppm or under is provided on the internal surface of a tubular YAG base of a discharge envelope. The mean particle size of the anti-corrosion layer is 20 .mu.m or over, and the mean particle size of the base is 15 .mu.m or under.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.