Abstract
Chlorine gas from a supply nozzle is mixed with the vapor of nickel chloride and the mixed gas is supplied from a supply nozzle into a hydrogen gas atmosphere in a reduction reactor at a reduction temperature of 900 to 1100.degree. C. The volume of chlorine gas to be mixed versus the vapor of nickel chloride is adjusted to a ratio of 0.01 to 0.5 moles per mole of the vapor of nickel chloride. The particle size of the nickel powder can be controlled appropriately, and also, uniformity of particle size, smoothability of surfaces of particles, and sphericity can be improved.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.