Patent · US Expired

Silicon steel sheet and method thereof

US6241829A · kind A · utility

1Cited by
8References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 9, 1999
Grant dateJun 5, 2001
Priority date
Expiry dateDec 9, 2019

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01F1/14775
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A silicon steel sheet contains 0.01 wt. % or less C, 4 to 10 wt. % Si, 0.5 wt. % or less Mn, 0.01 wt. % or less P, 0.01 wt. % or less S, 0.2 wt. % or less sol. Al, 0.01 wt. % or less N, 0.02 wt. % or less O and the balance being Fe. The silicon steel sheet has grain boundaries and carbides which are precipitated on the grain boundaries. The carbides have an area of 20% or less to an area of the grain boundaries. The steel sheet is cooled at a cooling speed of 5.degree. C./sec. or more in a temperature range of from 300 to 700.degree. C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.