Patent · US Expired

Pretreatment of chips before cooking

US6248208A · kind A · utility

2Cited by
9References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 2, 1995
Grant dateJun 19, 2001
Priority date
Expiry dateJun 2, 2015

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD21C1/06
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

The strength properties of chemical cellulose pulp (particularly kraft pulp) are improved by substituting a cold impregnation soak for conventional impregnation procedures. After steaming, wood chips are soaked in an alkaline liquid at a temperature of about 80-110.degree. C. (preferably 80-100.degree. C., or alternatively 90-105.degree. C.) for between one-half-72 hours (typically about 2-4 hours) at a pressure of about 0-15 bar (preferably about 1-5 bar), to dissolve at least about 8% of the wood (preferably about 10-20%) and at least about 15% of the lignin. The alkaline liquid used preferably contains sulfide (e.g. black liquor, green liquor, white liquor, or mixtures thereof), but almost any alkaline liquid having an alkali concentration of about 1.0 mole of NaOH/liter or less (typically about 0.75 m/l or less) is suitable. The wood chips are then raised to a cooking temperature of about 145-180.degree. C. and cooked to produce the cellulose chemical pulp. There may be an intermediate step, between soaking and raising the cooking temperature, of heating the wood chips to a temperature of about 110-150.degree. C. (preferably about 120-140.degree. C.) for about 10-90 minutes (pr…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.