Abstract
Water-cooling slabs by dipping to yield steel sheets with a minimum of scabs and uneven gloss, with their larger faces upside and underside, by water injection at a flow rate of 10-150 L/m.sup.2.multidot.min perpendicular or oblique to the underside of the slabs, with the position of water injection 30-500 mm away from the underside of the slabs.