Preparation of ultra-high-molecular-weight polyethylene
US6265504A · kind A · utility
26Cited by
6References
8Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Sep 22, 1999 |
| Grant date | Jul 24, 2001 |
| Priority date | — |
| Expiry date | Sep 22, 2019 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S526/943
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
An ultra-high-molecular-weight polyethylene (UHMWPE) is disclosed. The UHMWPE has a weight average molecular weight (Mw) greater than about 3,000,000 and molecular weight distribution less than about 5. A process for making the UHMWPE is also disclosed. The process is performed with a heteroatomic ligand-containing single-site catalyst in the presence of a non-alumoxane activator, but in the absence of an .alpha.-olefin, an aromatic solvent, and hydrogen.