Patent · US Expired

Process for preparation of hydroxyapatite coatings

US6280789A · kind A · utility

38Cited by
5References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 28, 1999
Grant dateAug 28, 2001
Priority date
Expiry dateJun 28, 2019

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2111/00844
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Coatings of scarcely crystalline carbonated hydroxyapatite are deposited on metallic or ceramic substrates, by immersing the substrates in a solution containing calcium phosphate and bicarbonate ions, with a molar ratio calcium/phosphate from 0.8 to 2 and a pH from 6.8 to 8.0. Subsequently, the solution is heated to 50-80.degree. C., thus raising the pH and causing a spontaneous deposition of carbonated hydroxyapatite on the substrates. The obtained coatings are highly biocompatible, osteoconductive, bioactive and biodegradable, and can be utilized in structures used for preparing orthopaedic and dental prostheses and implants.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.