Patent · US Expired

Hot-rolled steel strip and method of making it

US6284063A · kind A · utility

3Cited by
3References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 25, 1999
Grant dateSep 4, 2001
Priority date
Expiry dateFeb 25, 2019

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/008
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The invention concerns hot-rolled steel strip no more than 5 mm thick, optionally less than 2 mm thick, made of high-tensile steel, that contains 0.08%-0.25% carbon, 1.20% to 2.0% manganese, and 0.02% to 0.05% aluminum, and optionally up to 1.0% chromium, up to 0.1% copper, up to 0.5% molybdenum, up to 0.1% nickel, up to 0.009% nitrogen, up to 0.0025% B, and optionally a stoichiometric amount of titanium in relation to nitrogen. The steel strip has a greater than 95% martensitic structure, and a tensile strength of 800 to 1400 N/mm.sup.2.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.