Patent · US Expired

Method of preparing modified polyester bottle resins

US6284866A · kind A · utility

25Cited by
19References
23Claims
0Family size

Assignee

Inventor

Key dates

Filing dateDec 7, 1999
Grant dateSep 4, 2001
Priority date
Expiry dateDec 7, 2019

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/1397
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The present invention is a method of preparing a high molecular weight copolyester bottle resin that has excellent melt processing characteristics. The method includes the steps of reacting a diacid or diester component and a diol component to form modified polyethylene terephthalate, wherein diol component is present in excess of stoichiometric proportions. Together, the diacid or diester component and the diol component must include at least 7 percent comonomer. The remainder of the diacid component is terephthalic acid or dimethyl terephthalate and the remainder of the diol component is ethylene glycol. The modified polyethylene terephthalate is copolymerized in the melt phase to an intrinsic viscosity of between about 0.25 dl/g and 0.40 dl/g to thereby form a copolyester prepolymer. Thereafter the copolyester prepolymer is polymerized in the solid phase to form a high molecular weight bottle resin that has an intrinsic viscosity of at least about 0.70 dl/g, and a solid phase density of less than 1.413 g/cc.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.