Nylon 12, nylon composition, method for producing nylon 12, and tubular molded product using nylon 12
US6294644A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Mar 4, 1999 |
| Grant date | Sep 25, 2001 |
| Priority date | — |
| Expiry date | Mar 4, 2019 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/2969
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Disclosed is a member of nylon 12 having a relative viscosity of from 1.9 to 3.5 when measured in 98% sulfuric acid at a concentration of 10 g/dm.sup.3 and at 25.degree. C. and a melt flow rate of 0.1 g/10 min. or more when measured at 235.degree. C. under a load of 2,160 g, wherein said relative viscosity and said melt flow rate have a relationship of the following formula (I): EQU 2.87.times.10.sup.3 exp (-3.48 .eta..sub.r).ltoreq.MFR.ltoreq.3.25.times.10.sup.4 exp (-3.48 .eta..sub.r) (I) wherein .eta..sub.r is relative viscosity and MFR is melt flow rate. The nylon 12 has excellent extrusion moldability and creep characteristics, fatigue characteristics and the like mechanical properties and is suited for tubular molds. A nylon 12 composition comprising the nylon 12 having the above-described specific relationship between .eta..sub.r and MFR and a plasticizer is also disclosed.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.