Method for improving the dirt-resistance and gloss retention of a coalescent-free coating
US6303188A · kind A · utility
Assignee
Inventors
Key dates
| Filing date | Jul 8, 1994 |
| Grant date | Oct 16, 2001 |
| Priority date | — |
| Expiry date | Jul 8, 2014 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC09D133/062
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
A method for improving the dirt pick-up resistance and the retention of gloss on exposure to light of a dried coating formed from a coalescent-free aqueous coating composition is provided. The coalescent-free composition composition contains an aqueous emulsion-polymerized polymeric binder having a glass transition temperature from about -35 C. to about +25 C. with from about 2% to about 20%, by weight based on the weight of the polymeric binder, of at least one copolymerized ethylenically-unsaturated active methylene monomer.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.