Patent · US Expired

Process for working up steel slags and iron carriers for obtaining pig iron and environmentally safe slags

US6332910A · kind A · utility

5Cited by
4References
17Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMay 14, 1999
Grant dateDec 25, 2001
Priority date
Expiry dateMay 14, 2019

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/20
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

In a process for working up steel slags and iron carriers such as, e.g., electric furnace slags, converter slags, fine ores, dusts from steel production, mill scales for obtaining pig iron and environmentally safe slags, the volume ratio of molten slag to iron bath is chosen to be larger than 0.5 to 1 and, preferably, 0.8:1 to 1.5:1 and the slags are supplemented with SiO.sub.2 carriers such as, e.g., foundry sands, metallurgical sands and/or fine ores so as to adjust a slag basicity (CaO/SiO.sub.2) of between 1.0 and 1.8 and, preferably, 1.2 and 1.8 at an Al.sub.2 O.sub.3 content of between 10 and 25% by weight, based on the slag. In doing so, hot blast is top-blown and coal, optionally along with an inert gas and, in particular, nitrogen and, furthermore, optionally oxygen or hot air is blown through the iron bath.