Method of solidifying steel-making slag and material produced by the method
US6334885B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 13, 1999 |
| Grant date | Jan 1, 2002 |
| Priority date | — |
| Expiry date | Oct 13, 2019 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S106/01
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of solidifying a steel-making slag is performed by subjecting a mixture of a steel-making slag containing at least about 50% by weight of a powdery steel-making slag having a particle size not greater than about 5 mm and a substance containing at least about 30% by weight of SiO2 (e.g., a fly ash and/or the fine powder of a granulated blast furnace slag) to a hydration reaction. The resulting solidified material contains at least about 20% of a tobermorite phase, has high strength and is suitable as an inorganic material useful as a roadbed material, building and civil engineering materials, etc.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.