Patent · US Expired

Dielectric ceramic composition, capacitor using this and production method thereof

US6344427B1 · kind B1 · utility

16Cited by
4References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 29, 2000
Grant dateFeb 5, 2002
Priority date
Expiry dateNov 29, 2020

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/96
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A dielectric ceramic composition of the present invention is a mixture of barium titanate as a main component whose Ba/Ti molar ratio ranging from 1.001 to 1.05 and sub components comprising, at least 0.5 to 5.0 mol of Mg in the form of MgO, 0.1 to 3.0 mol of Dy in the form of Dy2O3, 0.01 to 0.4 mol of Mn in the form of Mn3O4, 0.01 to 0.26 mol of V in the form of V2O5, 0.3 to 3.5 mol of Si in the form of SiO2 and 0.01 to 3.0 mol of Al in the form of Al2O3 per 100 mol of the barium titanate. Even when external electrodes are made of base metal such as copper or the like, a multilayer capacitor whose dielectric layers are not reduced and have high insulation resistance can be obtained by using the dielectric ceramic composition of the present invention.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.