Abstract
A solid-solution strengthened superalloy weld composition, includes:about 10 to about 15 wt % Co;about 18 to about 22 wt % Cr;about 0.5 to about 1.3 wt % Al;about 3.5 to about 4.5 wt % Ta;about 1 to about 2 wt % Mo;about 13.5 to about 17.0 wt % W,up to about 0.08 wt % C;up to about 0.06 wt % Zr;up to about 0.015 wt % B;about 0.4 to about 1.2 wt % Mn;about 0.1 to about 0.3 wt % Si; andbalance Ni.