Abstract
A process for producing a poly(tetramethylene ether) glycol (PTMEG) or copolymer having a narrowed molecular weight ratio of 1.9 to 2.07 and a dispersity of 1.2 to 1.65 from a starting PTMEG or copolymer with a broader molecular weight distribution having a dispersity of 1.9 to 2.3 and a molecular weight ratio of 2.3 to 2.6 is provided by feeding the PTMEG or copolymer and an effective amount of an inert solvent to a stripping apparatus and stripping at a temperature of 150 to 220 degrees C. and a pressure of 0.5 to 5 mm of mercury.