Patent · US Expired

Enhancement of cement clinker yield

US6391105B1 · kind B1 · utility

7Cited by
4References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 16, 2001
Grant dateMay 21, 2002
Priority date
Expiry dateFeb 16, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S106/01
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The yield of cement clinker recovered from a kiln assembly is enhanced by feeding a particulate material comprising silica and an oxide of at least one of calcium and aluminum, for example, fly ash into contact with hot cement clinker; the fly ash melts to a partially fused material which chemically reacts with the hot clinker to produce a pyroprocessed cement clinker of crystalline hydraulic silicates; the extruder is added to the hot cement clinker downstream of the formation of the cement clinker, and suitably is added to the hot cement clinker at the upstream end of the cooler of the kiln assembly, or within the kiln, downstream of the burning zone, and more especially in the initial cooling zone at the discharge end of the kiln.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.