Process for preparing sintered body of aluminum titanate
US6403019B1 · kind B1 · utility
Inventors
Key dates
| Filing date | Nov 6, 2000 |
| Grant date | Jun 11, 2002 |
| Priority date | — |
| Expiry date | Dec 27, 2020 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC04B35/478
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The present invention provides a process for preparing a raw material powder for producing a sintered body of aluminum titanate comprising:pulverizing a mixture containing:(1) 100 parts by weight of aluminum titanate crystals pulverized until a maximum grain size of 30 to 50 &mgr;m is attained; and(2) 2 to 6 parts by weight of spinel crystals obtained by heating a mixture containing MgO and Al2O3 at 1250° C. to 1290° a molar ratio of MgO to Al2O3 being 1:0.95 to 1:1.05,said pulverizing being conducted by wet grinding process with a ball mill or cylinder mill.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.