Method for forming a thin film

US6440292B2 · kind B2 · utility

0Cited by
2References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 16, 2001
Grant dateAug 27, 2002
Priority date
Expiry dateMar 16, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A blended solution is made by melting LiOH.H2O into distilled water, and then, Co metallic powders are added into the blended solution to make a reactive solution. The reactive solution is charged into an autoclave, and held at a predetermined temperature. Then, a pair of platinum electrodes are set into the reactive solution, and a given voltage is applied between the pair of platinum electrode. As a result, a compound thin film, made of crystal LiCoO2 including Li element of the blended solution and Co element of the Co metallic powders, is synthesized on the platinum electrode constituting the anode electrode.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.