Process for producing hydrogenated &agr;-olefin-dicyclopentadiene copolymer, method for molding the same and optical material
US6476153B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Mar 9, 2001 |
| Grant date | Nov 5, 2002 |
| Priority date | — |
| Expiry date | May 1, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F210/02
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Process for producing a hydrogenated &agr;-olefin-dicyclopentadiene copolymer. The process includes a step of distilling of unreacted dicyclopentadiene or tetrahydrodicyclopentadiene which is a hydrogenated product of unreacted dicyclopentadiene from a mixture containing &agr;-olefin-dicyclopentadiene copolymer or its hydrogenated product in the presence of a high-boiling hydrocarbon solvent having a boiling point of 195 to 300° C. and an ignition point of 260° C. or more. Method for melt molding the hydrogenated &agr;-olefin-dicyclopentadiene copolymer is also proposed.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.