High temperature gaseous oxidation for passivation of austenitic alloys
US6488783B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Mar 30, 2001 |
| Grant date | Dec 3, 2002 |
| Priority date | — |
| Expiry date | Mar 30, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC23C8/02
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A method for forming a chromium-rich layer on the surface of a nickel alloy workpiece containing chromium includes heating the workpiece to a stable temperature of about 1100° C., and then exposing the workpiece to a gaseous mixture containing water vapor and one or more non-oxidizing gases for a short period of time. The process conditions are compatible with high temperature annealing and can be performed simultaneously with, or in conjunction with, high temperature annealing.