Abstract
Disclosed is a heat resistant steel casting, comprising C, 0.15-0.3%, Si, 0.1-0.30%, Mn, 0.01-0.1%, Cr, 2.0-2.5%, Mo, 0.3-0.8%, V, 0.23-0.3%, W, 1.6-2.6%, N, 0.005-0.03%, B, 0.001-0.004%, impurity elements including Ni not larger than 0.2%, P not larger than 0.03% and S not larger than 0.01%, B equivalent determined by B+0.5N given below being not larger than 0.02%, Mo equivalent determined by Mo+0.5W given below falling within a range of between 1.4% and 2.0%, and C equivalent determined by C+Mn/6+Si/24+Ni/40+Cr/5+Mo/14+V/14 given below being not smaller than 0.65%, and balance of iron wherein a precipitated phase consisting of a M23C6 carbide, a M7C3 carbide, and MX carbonitride is a texture finely precipitated in a matrix phase, and a ratio of the precipitated phase to the matrix phase falls within a range of between 0.6% and 1.0%.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.