Patent · US Expired

Lead-acid battery having tin in positive active material and silica in separator

US6495288B2 · kind B2 · utility

14Cited by
4References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 5, 2000
Grant dateDec 17, 2002
Priority date
Expiry dateJun 1, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49108
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

In a lead-acid battery, a positive active material includes tin in an amount of from not less than 0.2% to not more than 5% based on the weight thereof. The density of the positive active material after formation is from not less than 3.75 g/cc to not more than 5.0 g/cc. When the lead-acid battery is produced by a battery container formation, a time required between the injection of an electrolyte and the beginning of battery container formation is from not less than 0.1 hours to not more than 3 hours.