Patent · US Expired

Two step aging treatment for Ni-Cr-Mo alloys

US6544362B2 · kind B2 · utility

5Cited by
15References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 28, 2001
Grant dateApr 8, 2003
Priority date
Expiry dateJul 1, 2021

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C19/058
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A two step heat treatment for Ni—Cr—Mo alloys containing from 12% to 23.5% chromium provides higher yield strength, high tensile strength and other mechanical properties comparable to those observed in similar alloys age-hardened according to current practices. This treatment is done over a total time of not more than 50 hours. However, the treatment works for only those alloys having alloying elements present in amounts according to an equation here disclosed.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.