Patent · US Expired

Coating solution, method and kit for preparing the same, and method for water-repellent treatment using the same

US6564935B1 · kind B1 · utility

27Cited by
8References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 2, 2000
Grant dateMay 20, 2003
Priority date
Expiry dateNov 2, 2020

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC09K3/18
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A coating solution for water-repellent, oil-repellent, stain-proofing treatment is provided which does not become cloudy even if it is stored for a long time. Furthermore, a method for water-repellent, oil-repellent, stain-proofing treatment with the use of this coating solution is provided. The coating solution for water-repellent, oil-repellent, and stain-proofing treatment is obtained by mixing a first solution containing a fluoroalkyl group-containing silane and a second solution containing acid and a solvent, and this coating solution is used for the method for water-repellent, oil-repellent, stain-proofing treatment.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.