Patent · US Expired

Method of manufacturing molten metal iron

US6569223B2 · kind B2 · utility

13Cited by
16References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 29, 2001
Grant dateMay 27, 2003
Priority date
Expiry dateMar 29, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/134
  • WIPO fieldThermal processes and apparatus
  • WIPO sectorMechanical engineering

Abstract

A method of manufacturing a molten metal iron by charging a starting material at least comprising a carbonaceous reducing material and an iron oxide-containing material into a rotary hearth furnace, reducing under heating the charged starting material into a solid reducing iron, carburizing the metal iron in the solid reduced iron with the carbon ingredient in the carbonaceous reducing material, thereby melting the metal iron, separating the slag ingredient contained in the starting material by the melting, and discharging the molten metal alloy in the molten state as it is to the outside of the rotary hearth furnace for recovery, wherein a downward inclined surface is disposed at an angle 3 to 30° relative to the horizontal plane on the upper surface of a hearth of the rotary hearth furnace on which the starting material is placed, and the molten metal iron is discharged at the discharging position for the molten metal iron from the lowest portion of the inclined surface.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.