Aging treatment for Ni-Cr-Mo alloys
US6579388B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jun 28, 2001 |
| Grant date | Jun 17, 2003 |
| Priority date | — |
| Expiry date | Jul 31, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22F1/10
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A single step heat treatment for Ni-Cr-Mo alloys containing from 12% to 19% chromium and from 18% to 23% molybdenum provides higher yield strength, high tensile strength and other mechanical properties comparable to those observed in similar alloys age-hardened according to current practices. This treatment is done over a total time of at least 24 hours and preferably less than 50 hours. However, the treatment works for only those alloys having alloying elements present in amounts according to an equation here disclosed.