Patent · US Expired

FE-NI ALLOY HAVING HIGH STRENGTH AND LOW THERMAL EXPANSION, A SHADOW MASK MADE OF THE ALLOY, A BRAUN TUBE WITH THE SHADOW MASK, A LEAD FRAME MADE OF THE ALLOY AND A SEMICONDUCTOR ELEMENT WITH LEAD FRAME

US6592810B2 · kind B2 · utility

46Cited by
3References
21Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 19, 2001
Grant dateJul 15, 2003
Priority date
Expiry dateMar 19, 2021

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01L2924/0002
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Disclosed is an Fe—Ni alloy consisting of, by mass, 30 to 50% of Ni (or 27 to 47% Ni and not more than 22% Co), 0.005 to 0.1% of Nb, less than 0.01% of C, 0.002 to 0.02% of N, and the balance of Fe and inevitable impurities, wherein the equation“0.000013≦(% Nb)×(% N)≦0.002”,is fulfilled. In the alloy, preferably, the maximum grain size of compounds primarily containing Nb and nitrogen and other compounds primarily containing Nb and C is less than 0.5 &mgr;m, which can be observed at an fractional section of metal structure, and a total number of the compounds is not less than 50,000/mm2 at an fractional section. An average grain size of the alloy structure is not less than 10 by the crystal grain size number as defined in JIS G0551. The alloy may applied to shadow masks for the Braun tube and lead frames for semiconductor elements.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.