Patent · US Expired

Seal rings with improved friction and wear properties

US6609953B2 · kind B2 · utility

1Cited by
8References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 19, 2002
Grant dateAug 26, 2003
Priority date
Expiry dateDec 19, 2022

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/265
  • WIPO fieldMechanical elements
  • WIPO sectorMechanical engineering

Abstract

The present invention relates to a cemented carbide wear part with a wear surface with improved friction and wear properties. This has been obtained by providing the wear surface with a surface layer with a thickness of 0.5 &mgr;m to 25 &mgr;m, preferably 1 to 10 &mgr;m with an average WC grain size of less than 500 nm. The surface layer is obtained by lapping the wear surface with an abrasive disc for at least 10 minutes at 1000 to 3000 rpm at a pressure of 0.1 to 0.5 MPa preferably without any grinding media.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.